Simulation and analysis of stress in a Li-ion battery with a blended LiMn2O4 and LiNi0.8Co0.15Al 0.05O2 cathode

Dai, Yiling, Long Cai, and Ralph E. White. 2014. “Simulation and analysis of stress in a Li-ion battery with a blended LiMn2O4 and LiNi0.8Co0.15Al 0.05O2 cathode”. Journal of Power Sources 247: 365-76.

Abstract

Stress generation due to Li ion insertion into/extraction from LiMn 2O4 particles is studied with a mathematical model for a lithium ion battery with pure LiMn2O4 or mixed LiMn 2O4 and LiNi0.8Co0.15Al 0.05O2 cathode. The simulated stress profile in a pure LiMn2O4 electrode shows nonuniformity across the positive electrode. The cathode blended model predicts that the stress generated in the LiMn2O4 particles is reduced at the end of discharge due to adding LiNi0.8Co0.15Al0.05O2 to the cathode. The effect of the variation in the blend ratio on the stress generation is also investigated. © 2013 Elsevier B.V. All rights reserved.